用于測定各種毛織物和化纖、純紡、混紡、針織物的起毛起球狀況。
性能合:GB/T4802.1-1997《紡織品織物起球試驗(yàn)圓軌跡法》。
It is used for determining the condition of fabric pilling of all kinds of wool fabric, chemical fiber, qure fabric, blending fabric or knitting fabric.
Its property is in conformity with GB/T4802.1-1997《Textiles-Assessing the rate of pilling of fabric-Circular locus method》.
主要技術(shù)參數(shù):Main Technical Data
1、起毛起球圓軌跡Circular locus of fabric pilling圓軌跡Circular locus(Φ40mm)
2、試樣與磨臺相對運(yùn)轉(zhuǎn)速度
Relative motion speed between sample and rubbing table :60 r/min
3、試樣夾環(huán)內(nèi)徑ID of sample clamp ring 90 +/-0.5mm
4、試樣夾頭壓力Pressure of sample clamp 490cN,590cN,780cN
5、起毛起球次數(shù)Time of fabric pilling 5位
6、外形尺寸Outline size:L540*W250*H345mm